Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | typical value |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 13 % Show Material materials with Dehnung of 13 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | typical value |
Härte, Brinell | 23.0 °C | 207 [-] Show Material materials with Härte, Brinell of 207 [-] | in annealed condition: 197 |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | typical value |
Streckgrenze | 23.0 °C | 550 MPa Show Material materials with Streckgrenze of 550 MPa | |
Zugfestigkeit | 23.0 °C | 700 MPa Show Material materials with Zugfestigkeit of 700 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.1E-5 - 1.4E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.1E-5 - 1.4E-5 1/K | Typical for Chromium Molybdenum Steel |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel | |
Spezifische Wärmekapazität | 23.0 °C | 448 - 502 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel |
Wärmeleitfähigkeit | 23.0 °C | 36 - 43 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Chrom | 1.25 - 1.5 % Show Material materials with Chrom of 1.25 - 1.5 % | ||
Eisen | Balance | ||
Kohlenstoff | 0.12 - 0.18 % Show Material materials with Kohlenstoff of 0.12 - 0.18 % | ||
Mangan | 0.8 - 1.1 % Show Material materials with Mangan of 0.8 - 1.1 % | ||
Molybdän | 0.8 - 1 % Show Material materials with Molybdän of 0.8 - 1 % | ||
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % | max. | |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % | max. | |
Silizium | 0.2 % Show Material materials with Silizium of 0.2 % | max. | |
Vanadium | 0.2 - 0.3 % Show Material materials with Vanadium of 0.2 - 0.3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Pressure vessels, Wishbones, Uprights, Suspension components, Motorsport applications, Track and push rods, Rocket motor casings, Roll cages, Aerospace |