Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | typical value |
Abmessung
Property | Value | Comment |
---|---|---|
Dicke | 200 mm Show Material materials with Dicke of 200 mm | max. |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 40 % Show Material materials with Dehnung of 40 % | min., A5.65 |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | typical value |
Härte, Vickers | 23.0 °C | 270 - 300 [-] Show Material materials with Härte, Vickers of 270 - 300 [-] | |
Kerbschlagenergie | 23.0 °C | 180 J Show Material materials with Kerbschlagenergie of 180 J | min. |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | typical value |
Streckgrenze | 23.0 °C | 600 - 800 MPa Show Material materials with Streckgrenze of 600 - 800 MPa | |
Zugfestigkeit | 23.0 °C | 900 - 1050 MPa Show Material materials with Zugfestigkeit of 900 - 1050 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Chrom | 18 - 20 % Show Material materials with Chrom of 18 - 20 % | max. | |
Eisen | Balance | ||
Kohlenstoff | 0.12 % Show Material materials with Kohlenstoff of 0.12 % | max. | |
Mangan | 9 - 11 % Show Material materials with Mangan of 9 - 11 % | ||
Molybdän | 1 % Show Material materials with Molybdän of 1 % | max. | |
Nickel | 1 % Show Material materials with Nickel of 1 % | max. | |
Phosphor | 0.06 % Show Material materials with Phosphor of 0.06 % | max. | |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % | max. | |
Silizium | 1 % Show Material materials with Silizium of 1 % | max. | |
Stickstoff | 0.4 - 0.65 % Show Material materials with Stickstoff of 0.4 - 0.65 % | max |