Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | typical value |
Abmessung
Property | Value |
---|---|
Dicke | 16 - 250 mm Show Material materials with Dicke of 16 - 250 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 11 - 13 % Show Material materials with Dehnung of 11 - 13 % | min., A5.65 |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | typical value |
Härte, Brinell | 23.0 °C | 248 [-] Show Material materials with Härte, Brinell of 248 [-] | max. |
Kerbschlagenergie | 23.0 °C | 30 - 45 J Show Material materials with Kerbschlagenergie of 30 - 45 J | min. |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | typical value |
Streckgrenze | 23.0 °C | 700 - 950 MPa Show Material materials with Streckgrenze of 700 - 950 MPa | min. |
Zugfestigkeit | 23.0 °C | 900 - 1350 MPa Show Material materials with Zugfestigkeit of 900 - 1350 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.3E-5 1/K | typical value |
Spezifische Wärmekapazität | 23.0 °C | 470 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 470 J/(kg·K) | typical value |
Wärmeleitfähigkeit | 23.0 °C | 39 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 39 W/(m·K) | typical value |
Elektrisch
Property | Value | Comment |
---|---|---|
Specific Electrical conductivity | 7.8 % IACS Show Material materials with Specific Electrical conductivity of 7.8 % IACS | typical value |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Chrom | 2.8 - 3.3 % Show Material materials with Chrom of 2.8 - 3.3 % | ||
Eisen | Balance | ||
Kohlenstoff | 0.29 - 0.36 % Show Material materials with Kohlenstoff of 0.29 - 0.36 % | ||
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % | max. DIN EN ISO 683-17: 0.1-0.4 | |
Mangan | 0.4 - 0.7 % Show Material materials with Mangan of 0.4 - 0.7 % | ||
Molybdän | 0.7 - 1 % Show Material materials with Molybdän of 0.7 - 1 % | DIN EN ISO 683-17: 0.7-1.2 | |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % | max. DIN EN ISO 683-17 | |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % | max. | |
Schwefel | 0.035 % Show Material materials with Schwefel of 0.035 % | max. DIN EN ISO 683-17: 0.015 | |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % | max. DIN EN ISO 683-17: 0.1-0.4 | |
Vanadium | 0.15 - 0.25 % Show Material materials with Vanadium of 0.15 - 0.25 % |