Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | typical value |
Abmessung
Property | Value |
---|---|
Dicke | 16 - 100 mm Show Material materials with Dicke of 16 - 100 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 10 - 12 % Show Material materials with Dehnung of 10 - 12 % | min., A5.65 |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | typical value |
Flächenreduzierung | 23.0 °C | 30 - 40 % Show Material materials with Flächenreduzierung of 30 - 40 % | min. |
Härte, Brinell | 23.0 °C | 217 [-] Show Material materials with Härte, Brinell of 217 [-] | max. in soft annealed condition |
Kerbschlagenergie | 23.0 °C | 15 - 30 J Show Material materials with Kerbschlagenergie of 15 - 30 J | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | typical value |
Streckgrenze | 23.0 °C | 685 - 885 MPa Show Material materials with Streckgrenze of 685 - 885 MPa | |
Zugfestigkeit | 23.0 °C | 880 - 1270 MPa Show Material materials with Zugfestigkeit of 880 - 1270 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.33E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.33E-5 1/K | Typical for Manganese Steel |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Manganese Steel | |
Spezifische Wärmekapazität | 23.0 °C | 510 - 553 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 510 - 553 J/(kg·K) | Typical for Manganese Steel |
Wärmeleitfähigkeit | 23.0 °C | 14 - 16 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 14 - 16 W/(m·K) | Typical for Manganese Steel |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Eisen | Balance | ||
Kohlenstoff | 0.38 - 0.45 % Show Material materials with Kohlenstoff of 0.38 - 0.45 % | ||
Mangan | 1.6 - 1.9 % Show Material materials with Mangan of 1.6 - 1.9 % | ||
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % | max. | |
Schwefel | 0.035 % Show Material materials with Schwefel of 0.035 % | max. | |
Silizium | 0.15 - 0.35 % Show Material materials with Silizium of 0.15 - 0.35 % | ||
Vanadium | 0.07 - 0.12 % Show Material materials with Vanadium of 0.07 - 0.12 % |