Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8 g/cm³ Show Material materials with Dichte of 8 g/cm³ |
Abmessung
Property | Value | Comment |
---|---|---|
Dicke | 50 mm Show Material materials with Dicke of 50 mm | max. |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 30 % Show Material materials with Dehnung of 30 % | min., A5.65 |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | typical value |
Kerbschlagenergie | 23.0 °C | 60 J Show Material materials with Kerbschlagenergie of 60 J | min. |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | typical value |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Austenitic Stainless Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 210 MPa Show Material materials with Streckgrenze Rp 0,2 of 210 MPa | min. |
Streckgrenze Rp0,1 | 23.0 °C | 235 MPa Show Material materials with Streckgrenze Rp0,1 of 235 MPa | min. |
Zugfestigkeit | 23.0 °C | 480 MPa Show Material materials with Zugfestigkeit of 480 MPa | min. |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 1.65E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.65E-5 1/K | mean value between 20°C and the mentioned temperature |
200.0 °C | 1.75E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.75E-5 1/K | mean value between 20°C and the mentioned temperature | |
300.0 °C | 1.85E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.85E-5 1/K | mean value between 20°C and the mentioned temperature | |
Schmelzpunkt | 1230 - 1480 °C Show Material materials with Schmelzpunkt of 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Spezifische Wärmekapazität | 23.0 °C | 500 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 500 J/(kg·K) | |
Wärmeleitfähigkeit | 50.0 °C | 15 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 15 W/(m·K) | |
100.0 °C | 16 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 16 W/(m·K) | ||
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 8.5E-7 Ω·m Show Material materials with spezifischer Widerstand of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Chrom | 19 - 21 % Show Material materials with Chrom of 19 - 21 % | ||
Eisen | Balance | ||
Kohlenstoff | 0.025 % Show Material materials with Kohlenstoff of 0.025 % | max. | |
Kupfer | 0.5 - 1.5 % Show Material materials with Kupfer of 0.5 - 1.5 % | ||
Mangan | 2 % Show Material materials with Mangan of 2 % | max | |
Molybdän | 6 - 7 % Show Material materials with Molybdän of 6 - 7 % | ||
Nickel | 24 - 26 % Show Material materials with Nickel of 24 - 26 % | ||
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % | max. | |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % | max. | |
Silizium | 1 % Show Material materials with Silizium of 1 % | max. | |
Stickstoff | 0.1 - 0.25 % Show Material materials with Stickstoff of 0.1 - 0.25 % |