Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.3 g/cm³ Show Material materials with Dichte of 1.3 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegemodul | 23.0 °C | 1.7 GPa Show Material materials with Biegemodul of 1.7 GPa | ASTM D790 | ||
Dehnung | 23.0 °C | 60 % Show Material materials with Dehnung of 60 % | ASTM D638 | ||
Druckfestigkeit | 23.0 °C | 98.9 MPa Show Material materials with Druckfestigkeit of 98.9 MPa | ASTM D695 | ||
Elastizitätsmodul | 23.0 °C | 2.34 GPa Show Material materials with Elastizitätsmodul of 2.34 GPa | ASTM D638 | ||
Elongation at yield | 23.0 °C | 7.2 % Show Material materials with Elongation at yield of 7.2 % | ASTM D638 | ||
Flexural yield strength | 23.0 °C | 91 MPa Show Material materials with Flexural yield strength of 91 MPa | ASTM D790 | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 690 J/m Show Material materials with Impact strength, Izod notched, ASTM of 690 J/m | ASTM D256 | ||
Kompressionsmodul | 23.0 °C | 1.73 MPa Show Material materials with Kompressionsmodul of 1.73 MPa | ASTM D695 | ||
Poissonzahl | 23.0 °C | 0.42 [-] Show Material materials with Poissonzahl of 0.42 [-] | ASTM E132 | ||
Scherfestigkeit | 23.0 °C | 62.7 MPa Show Material materials with Scherfestigkeit of 62.7 MPa | ASTM D732 | ||
Streckgrenze | 23.0 °C | 69.6 MPa Show Material materials with Streckgrenze of 69.6 MPa | ASTM D638 | ||
Zugfestigkeit | 23.0 °C | 69.6 MPa Show Material materials with Zugfestigkeit of 69.6 MPa | ASTM D638 | ||
Impact strength, Izod unnotched, ASTM | No Break, ASTM D256 |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Glasübergangstemperatur | 220 °C Show Material materials with Glasübergangstemperatur of 220 °C | ASTM E1356 | |||
Heat deflection temperature, 0.45 MPa | 214 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 214 °C | ASTM D648 | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 5.6E-5 1/K | ASTM D696 | ||
Wärmeleitfähigkeit | 23.0 °C | 0.35 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 0.35 W/(m·K) | ASTM C177 | ||
Entflammbarkeit | V-0 UL94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante | 23.0 °C | 3.44 [-] Show Material materials with Dielektrizitätskonstante of 3.44 [-] | ASTM D150, at 60 Hz |
Durchschlagfestigkeit | 23.0 °C | 14 kV/mm Show Material materials with Durchschlagfestigkeit of 14 kV/mm | ASTM D149 |
spezifischer Widerstand | 23.0 °C | 9.00E+13 Ω·m Show Material materials with spezifischer Widerstand of 9.00E+13 Ω·m |
Optisch
Property | Value | Comment |
---|---|---|
Brechungsindex | 1.67 [-] Show Material materials with Brechungsindex of 1.67 [-] | ASTM D542 |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace Applications, Connectors,Dental Applications, Food Service Applications, Hospital Goods, Medical Devices,Medical/Healthcare Applications, Plumbing Parts,Surgical Instruments | |
Color | Transparent, Opaque, Black, Grey, Violet, Brown, Red, Yellow, Orange, Green, Violet | |
Processing methods | Blow Molding, Extrusion, Film Extrusion, Profile Extrusion, Sheet Extrusion, Thermoforming - Injection Molding: Drying Temperature: 149°C, Drying Time: 2.5 hr, Rear Temperature: 321°C, Middle Temperature: 349°C, Front Temperature: 349°C, Melt Temperature: 343-388°C, Mold Temperature: 138-163°C, Back Pressure: 0.345-0.689 MPa, Screw Compression Ratio: 2.2:1 |