Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1 g/cm³ Show Material materials with Dichte of 1 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 2.05 GPa Show Material materials with Biegemodul of 2.05 GPa | ISO 178 | 2 mm/min, 64mm |
Dehnung | 23.0 °C | 26.7 % Show Material materials with Dehnung of 26.7 % | ISO 527 | 50 mm/min |
Elastizitätsmodul | 23.0 °C | 1.96 GPa Show Material materials with Elastizitätsmodul of 1.96 GPa | ISO 527 | 1 mm/min |
Elongation at yield | 23.0 °C | 4.6 % Show Material materials with Elongation at yield of 4.6 % | ISO 527 | 50 mm/min |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 4 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 4 kJ/m² | ISO 179/1eA |
Streckgrenze | 23.0 °C | 25 MPa Show Material materials with Streckgrenze of 25 MPa | ISO 527 | 50 mm/min |
Zugfestigkeit | 23.0 °C | 18 MPa Show Material materials with Zugfestigkeit of 18 MPa | ISO 527 | 50 mm/min, 1A |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 62 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 62 °C | ISO 75-1&2 | 1.8 MPa | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 5.6E-5 1/K | ISO 11359-2 | -30°C to 100°C |
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 1.16E-4 1/K Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 1.16E-4 1/K | ISO 11359-2 | -30°C to 100°C |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 23 g/10min Show Material materials with Schmelzmassenflussrate of 23 g/10min | ISO 1133 | 230°C/2.16 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Load Floor | |
Fillers | Mineral Powder | |
Processing methods | Drying Temperature: 80-100°C, Drying Time: 2-4hrs, Melt Temperature: 210-270°C, Nozzle Temperature: 210-270°C, Front - Zone 3 Temperature: 210-270°C, Middle - Zone 2 Temperature: 200-250°C, Rear - Zone 1 Temperature: 190-230°C, Mold Temperature: 15-60°C, Back Pressure: 1-1.5MPa |