Elongation at yield: 4.6 %

Quick Comparison

Polybutylenterephthalat (PBT)

Crastin® S650FR NC010

Polymermischung (Blend)

XENOY™ Resin 5720U

Polyamide 66 (PA66)

Zytel® 101L BKB009

Polyamide 410 (PA410)

EcoPaXX® Q170E-H

Geliefert von:

DSM Engineering Materials

Polyamide 410 (PA410)

EcoPaXX® Q170E-H B-MB

Geliefert von:

DSM Engineering Materials

Polypropylen (PP)

SABIC® PPcompound 7727