Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.92 g/cm³ Show Material materials with Dichte of 0.92 g/cm³ | ASTM D1505 |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 120 °C Show Material materials with Schmelzpunkt of 120 °C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante | 23.0 °C | 2.25 [-] Show Material materials with Dielektrizitätskonstante of 2.25 [-] | ASTM D150 |
Durchschlagfestigkeit | 23.0 °C | 37 kV/mm Show Material materials with Durchschlagfestigkeit of 37 kV/mm | ASTM D150 |
Verlustfaktor | 23.0 °C | 7E-4 [-] Show Material materials with Verlustfaktor of 7E-4 [-] | ASTM D150 |
Technological properties
Property | ||
---|---|---|
Application areas | Wire & cable |