Polyvinylidenefluoride (PVDF)
Kynar Superflex® 2500-20Geliefert von:
Arkema: High Performance PolymersPolyamide 66 (PA66)
Zytel® 79G13L NC010Polyamide 66 (PA66)
Zytel® 70G35EF BK538Polymermischung (Blend)
Zytel® 74G33W BK196Polyamide 66 (PA66)
Zytel® FR70G25V0 NC010Polyamide 66 (PA66)
Zytel® FR95G25V0NH NC010Polybutylenterephthalat (PBT)
Crastin® SK612SF NC010Polyvinylidenefluoride (PVDF)
Kynar Superflex® 2500-25Geliefert von:
Arkema: High Performance PolymersPolyethylen (PE)
SABIC® LLDPE 320BTPolyethylen (PE)
SABIC® LLDPE 320NT