Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materialien
Categories
Sie sind nicht angemeldet
Categories
Metalllieferanten finden
List Your Company
Case Studies
Tools
Über uns
SABIC® LLDPE 320NT
SABIC® 320NT is an ethylene-butene copolymer designed for wire and cable application. it is designed for high speed cable extrusion line, product use 320NT has excellent cable outlook, compare to the other polyethylene, 320NT is designed to reduce the use of additive during compounding, suggest the customer to optimize the silane and peroxide amount for 320NT based material, suitable for one-step silane crosslinking low voltage power cable insulation. 320NT contains no slip and no antiblock.
Diese Materialdaten wurden von Matmatch zur Verfügung gestellt
All categories
Let us help you find the best supplier!
Blow Moulding: History, Process, and Types
Difference between Biodegradable, Compostable, and Degradable
Fluoropolymers - The non-stick coating discovered by accident
LDPE vs HDPE: Properties, Production and Applications
PETG vs PLA
Polycarbonate (PC)
Polyether Ether Ketone (PEEK): Properties, Production, and Applications
Polyethylene (PE)
Polyethylene Wax: Uses and Properties
Polyimide: Properties, Processing, and Applications
Polypropylene: Properties, Processing, and Applications
Polytetrafluoroethylene (PTFE): Properties, Processing, and Applications
Polyvinyl Chloride (PVC): Properties, Processing, and Applications
Polyvinylidene Fluoride (PVDF): Properties, Production, & Applications
Styrene: Properties, Processing, and Applications
Thermoplastics vs. Thermosetting Polymers: Properties, Processing and Applications
What is Hostaform® M90XAP® POM?
What is Nylatron® GS?
What is Radel® R-5100?
What is Rilsan and what is it used for?
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationAllgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.92 g/cm³ Show Material materials with Dichte of 0.92 g/cm³ | ASTM D1505 |
Thermisch
Property | Value | Comment |
---|---|---|
Schmelzpunkt | 120 °C Show Material materials with Schmelzpunkt of 120 °C | SABIC method |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante | 23.0 °C | 2.25 [-] Show Material materials with Dielektrizitätskonstante of 2.25 [-] | ASTM D150 |
Durchschlagfestigkeit | 23.0 °C | 37 kV/mm Show Material materials with Durchschlagfestigkeit of 37 kV/mm | ASTM D150 |
Verlustfaktor | 23.0 °C | 7E-4 [-] Show Material materials with Verlustfaktor of 7E-4 [-] | ASTM D150 |
Technological properties
Property | ||
---|---|---|
Application areas | Wire & cable |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
UNTERNEHMEN
KONTAKTIEREN SIE UNS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.