Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.45 g/cm³ Show Material materials with Dichte of 1.45 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 215 MPa Show Material materials with Biegefestigkeit of 215 MPa | ISO 178 |
Biegemodul | 23.0 °C | 10.5 GPa Show Material materials with Biegemodul of 10.5 GPa | ISO 178 |
Dehnung | 23.0 °C | 2.2 % Show Material materials with Dehnung of 2.2 % | ISO 527-1/-2 |
Elastizitätsmodul | 23.0 °C | 10.8 GPa Show Material materials with Elastizitätsmodul of 10.8 GPa | ISO 527-1/-2 |
Poissonzahl | 23.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | |
Schlagfestigkeit, Charpy gekerbt | -6.0 °C | 6 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | ISO 179/1eA |
23.0 °C | 6 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -6.0 °C | 40 kJ/m² Show Material materials with Schlagzähigkeit, Charpy ungekerbt of 40 kJ/m² | ISO 179/1eU |
23.0 °C | 46 kJ/m² Show Material materials with Schlagzähigkeit, Charpy ungekerbt of 46 kJ/m² | ISO 179/1eU | |
Zugfestigkeit | 23.0 °C | 148 MPa Show Material materials with Zugfestigkeit of 148 MPa | ISO 527-1/-2 |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 283 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 283 °C | ISO 75-1/-2 | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.7E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.7E-5 1/K | ISO 11359-1/-2 | 23 - 55°C | ||
Relative temperature index, electrical | 140 °C Show Material materials with Relative temperature index, electrical of 140 °C | UL 746B | 120mil | |||
Relative temperature index, mechanical impact | 120 °C Show Material materials with Relative temperature index, mechanical impact of 120 °C | UL 746B | 120mil | |||
Relative temperature index, mechanical strength | 130 °C Show Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | 120mil | |||
Schmelzpunkt | 310 °C Show Material materials with Schmelzpunkt of 310 °C | ISO 11357-1/-3 | first heat | |||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 1.2E-4 1/K Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 1.2E-4 1/K | ISO 11359-1/-2 | 55 - 160°C | ||
Entflammbarkeit | Burning Behav. at thickness h: V-0 class, Thickness tested: 0.4 mm, UL recognition: yes - |
Elektrisch
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber | |
Processing methods | Drying Recommended: yes, Drying Temperature: 100°C, Drying Time, Dehumidified Dryer: 6-8h, Processing Moisture Content: ≤0.1%, Min. melt temperature: 320°C, Max. melt temperature: 325°C, Min. mold temperature: 90°C, Max. mold temperature: 130°C |