Polyethylenterephthalat (PET)
Rynite® FR530 NC010Polyamide 6T (PA6T)
Zytel® HTNFR52G30BL NC010Copolyamide 6T/6I/66 (PA6T/6I/66)
RADILON AESTUS T1 RV330RG 3900 BKGeliefert von:
RadiciGroup High Performance PolymersPolyethylenterephthalat (PET)
Rynite® FR530 BK507Polyamide 6T (PA6T)
Zytel® HTNLTFR52G30NH BL662Polyamide 6T (PA6T)
Zytel® HTN51G35HSLR BK420Copolyamide 6T/66 (PA6T/66)
RADILON AESTUS T2 RV350W 333 BKGeliefert von: