Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.41 g/cm³ Show Material materials with Dichte of 1.41 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 2.9 % Show Material materials with Dehnung of 2.9 % | ISO 527-1/-2 |
Elastizitätsmodul | 23.0 °C | 11 GPa Show Material materials with Elastizitätsmodul of 11 GPa | ISO 527-1/-2 |
Poissonzahl | 23.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 12 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 12 kJ/m² | ISO 179/1eA |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 70 kJ/m² Show Material materials with Schlagzähigkeit, Charpy ungekerbt of 70 kJ/m² | ISO 179/1eU |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 12 kJ/m² Show Material materials with Schlagzähigkeit, Izod ungekerbt of 12 kJ/m² | ISO 180/1A |
Zugfestigkeit | 23.0 °C | 210 MPa Show Material materials with Zugfestigkeit of 210 MPa | ISO 527-1/-2 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Glasübergangstemperatur | 70 °C Show Material materials with Glasübergangstemperatur of 70 °C | ISO 11357-1/-2 | 18°F/min | |
Heat deflection temperature, 0.45 MPa | 260 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 260 °C | ISO 75-1/-2 | |
Heat deflection temperature, 1.80 MPa | 254 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 254 °C | ISO 75-1/-2 | |
Schmelzpunkt | 263 °C Show Material materials with Schmelzpunkt of 263 °C | ISO 11357-1/-3 | 18°F/min | |
Entflammbarkeit | Oxygen index: 21 %, FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Material materials with Volume resistivity of 1.00E+15 Ω·cm | min. | IEC 62631-3-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 35% Glass Fiber | |
Processing methods | Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 295°C, Min. melt temperature: 285°C, Max. melt temperature: 305°C, Max. screw tangential speed: 0.2m/s, Mold Temperature Optimum: 100°C, Min. mold temperature: 70°C, Max. mold temperature: 120°C, Hold pressure range: 50-100MPa, Hold pressure time: 3s/mm, Ejection temperature: 210°C |