Heat deflection temperature, 0.45 MPa: 260 °C

Quick Comparison

Polyamide 66 (PA66)

Zytel® 79G13L NC010

Polyamide 66 (PA66)

Akulon® S223-HG6

Geliefert von:

DSM Engineering Materials

Polyamide 66 (PA66)

Zytel® 70G35HSLX BK357

Polyamide 66 (PA66)

Zytel® 79G13HSL NC010

Polyamide 66 (PA66)

Akulon® S223-HG7

Geliefert von:

DSM Engineering Materials

Polyamide 66 (PA66)

Akulon® HR-HG6

Geliefert von:

DSM Engineering Materials

Polyamide 66 (PA66)

Zytel® 70G30L NC010

Polyamide 66 (PA66)

Akulon® S223-G6

Geliefert von:

DSM Engineering Materials

Polyamide 66 (PA66)

Akulon® HR-HG7

Geliefert von:

DSM Engineering Materials

Other Polyamide (PA)

Zytel® FG70G30HSR3 BK309

Polyamide 66 (PA66)

Zytel® 70G35HSRX BK099

Polyamide 66 (PA66)

Zytel® 70G35HSL BK039B

Polyamide 66 (PA66)

Zytel® 70G33HSL BK083

Polyamide 66 (PA66)

Novamid® 3021GH30 BK629

Geliefert von:

DSM Engineering Materials

Polyamide 66 (PA66)

Akulon® M-1016

Geliefert von:

DSM Engineering Materials

Polyamide 66 (PA66)

Akulon® S223-HPG5

Geliefert von:

DSM Engineering Materials

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RFL33

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RFL36S

Geliefert von:

Sabic