Mechanisch
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Seawater trunking, fasteners, tubes, fittings and other components for seawater condensors;Chemical processing: Evaporator, distillation and heat-exchanger equipment including desalination plant and sugar refineries;General engineering: Washers, fasteners and pins | |
Corrosion properties | Very good fresh water and sea water corrosion resistance |