Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 12 - 18 % Show Material materials with Dehnung of 12 - 18 % |
Streckgrenze | 23.0 °C | 210 - 270 MPa Show Material materials with Streckgrenze of 210 - 270 MPa |
Zugfestigkeit | 23.0 °C | 440 - 460 MPa Show Material materials with Zugfestigkeit of 440 - 460 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 1 % Show Material materials with Aluminium of 1 % |
Eisen | 0.7 % Show Material materials with Eisen of 0.7 % |
Kupfer | 58 % Show Material materials with Kupfer of 58 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Zink | 39 % Show Material materials with Zink of 39 % |
Zinn | 0.6 % Show Material materials with Zinn of 0.6 % |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Marine hardware and fasteners;Other: Gas valves and fittings, fasteners, pump trim, gears, locks, heavy-duty electrical connectors, transmission components, safety tools and decorative metalwork | |
Corrosion properties | Good corrosion resistance | |
General machinability | Good machinability |