Global Steel Wire, S.A. is the Celsa Group company engaged in manufacturing wire rod in an extensive range of steels and dimensions, which have been progressively expanded in order to be increasingly present in higher technology sectors.
Headquarters
Santander,Cantabria, Spain
Type
Manufacturer and Processor
Certifications
IATF 16949
, ISO 9001
, OHSAS 18001
, ISO 14001
Grade | Shape | ||
---|---|---|---|
EN CW508L | Bar, Profile | EN CW508L, EN CuZn37 | EN 12164, EN 12165, EN 1216, EN 12167 |
EN CW509L | Bar, Profile | EN CW509L, EN CuZn40 | EN 12164, EN 12165, EN 1216, EN 12167 |
EN CW602N | Bar, Profile | EN CW602N, EN CuZn36Pb2As | EN 12164, EN 12165, EN 1216, EN 12167 |
EN CW603N | Bar, Profile | EN CW603N, EN CuZn36Pb3 | EN 12164, EN 12165, EN 1216, EN 12167 |
EN CW608N | Bar, Profile | EN CW608N, EN CuZn38Pb2 | EN 12164, EN 12165, EN 1216, EN 12167 |
EN CW612N | Bar, Profile | EN CW612N, EN CuZn39Pb2 | EN 12164, EN 12165, EN 1216, EN 12167 |
EN CW614N | Bar, Profile | EN CW614N, EN CuZn39Pb3 | EN 12164, EN 12165, EN 1216, EN 12167 |
EN CW617N | Bar, Profile | EN CW617N, EN CuZn40Pb2 | EN 12164, EN 12165, EN 1216, EN 12167 |
EN CW624N | Bar, Profile | EN CW624N, EN CuZn43Pb2Al | EN 12164, EN 12165, EN 1216, EN 12167 |
EN CW721R | Bar, Profile | EN CW721R, EN CuZn40Mn1Pb1AlFeSn | EN 12164, EN 12165, EN 1216, EN 12167 |