Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 7 - 10 % Show Material materials with Dehnung of 7 - 10 % |
Streckgrenze | 23.0 °C | 540 - 590 MPa Show Material materials with Streckgrenze of 540 - 590 MPa |
Zugfestigkeit | 23.0 °C | 780 - 830 MPa Show Material materials with Zugfestigkeit of 780 - 830 MPa |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace: Landing gear;Other: Heat exchanger, evaporator, condenser and desalination plant and equipment, high strength fasteners, pump and valve trim, landing gear, heavy duty bearing bushes, general engineering applications such as shafts, axles, pins and other fasteners | |
Corrosion properties | High corrosion resistance | |
General machinability | Good machining | |
Hot forming | Good hot foming |