Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 12 - 25 % Show Material materials with Dehnung of 12 - 25 % |
Streckgrenze Rp 0,2 | 23.0 °C | 380 - 420 MPa Show Material materials with Streckgrenze Rp 0,2 of 380 - 420 MPa |
Zugfestigkeit | 23.0 °C | 280 - 500 MPa Show Material materials with Zugfestigkeit of 280 - 500 MPa |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Marine hardware and fasteners;Power generation: Electrical springs and contacts;Other: Pump and valve spindles, fasteners, sleeve bushings, springs, shafts, flanges, architectural and decorative components, lock washers, spring washers and masonry fixings | |
Cold Forming | Good cold formability | |
Corrosion properties | Very good corrosion resistance | |
General machinability | Machinability Rating: 20 |