Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 12 - 18 % Show Material materials with Dehnung of 12 - 18 % |
Härte, Vickers | 23.0 °C | 150 - 170 [-] Show Material materials with Härte, Vickers of 150 - 170 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 380 - 440 MPa Show Material materials with Streckgrenze Rp 0,2 of 380 - 440 MPa |
Zugfestigkeit | 23.0 °C | 460 - 525 MPa Show Material materials with Zugfestigkeit of 460 - 525 MPa |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Marine hardware and instrument components;Power generation: Electrical springs and contacts;Other: Gaskets, instrument components, architectural and decorative purposes, components in paper and textile manufacturing plants, wire, flanges and masonry fixings | |
Corrosion properties | Very good corrosion resistance | |
General machinability | Machinability Rating: 20 |