Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 15 - 20 % Show Material materials with Dehnung of 15 - 20 % |
Streckgrenze Rp 0,2 | 23.0 °C | 300 - 450 MPa Show Material materials with Streckgrenze Rp 0,2 of 300 - 450 MPa |
Zugfestigkeit | 23.0 °C | 450 - 600 MPa Show Material materials with Zugfestigkeit of 450 - 600 MPa |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Fasteners, nuts, bolts, thrust washers, lock washers, pinions, bearings, bushes and connecting rods;Automotive: Heavy duty bearings, bushes and gears, driving pinions, axels, hinges, engine valve guides and seats;Other: Components for the chemical, textile, papermaking and other manufacturing industries including press guide bushes, chemical hardware and pump components | |
Corrosion properties | High corrosion resistance | |
General machinability | Machinability Rating: 20 |