Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materialien
Categories
Sie sind nicht angemeldet
Categories
Metalllieferanten finden
List Your Company
Case Studies
Tools
Über uns
BS C110 / Cu-OFE Oxygen-free Copper
C110 (Cu-OFE) is the purest grade of oxygen-free copper, with a 99.99% copper content. With much tighter limits on impurities than other grades, C110 offers the highest electrical and thermal conductivity values available from a commercially available copper alloy and is not susceptible to embrittlement when hardened. Specified for electronic applications requiring freedom from harmful impurities and oxide which can impair and contaminate electronic devices, C110 also has high ductility. It shows the following features and properties:
Diese Materialdaten wurden von Matmatch zur Verfügung gestellt
All categories
Suppliers with similar grades
Healthcare
Medizinische Ausrüstung
Radiografische Ausrüstung
Flüssigkeitssysteme
Vakuumtechnologie
Herstellung
Schweißung
Glas-Metall-Dichtungen
Oberflächenbearbeitung und -beschichtung
Anoden
Chemie-Industrie
Anlagen für die Chemieindustrie
Wärmetauscher
Energie
Treibstoffzellen
Elektrotechnik
Semiconducting Materials
Komponenten für Elektrogeräte
Magnetische Komponenten
Elektrisches Zubehör
Schalter
Elektronik
Elektronische Rohre
Kommunikation
Telecom Accessories
Waveguides
Properties of Copper
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationChemical properties
Property | Value | Comment |
---|---|---|
Kupfer | 99.99 % Show Material materials with Kupfer of 99.99 % | min. |
Technological properties
Property | ||
---|---|---|
Application areas | General: Components for vacuum devices, switches, interrupters, deposition units, components for superconductive magnets, electron tubes including anodes, fins and collectors, glass-to-metal seals, wave guide tubes and linear accelerators | |
Cold Forming | Easily cold worked |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
UNTERNEHMEN
KONTAKTIEREN SIE UNS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.