Property | ||
---|---|---|
Application areas | Aerospace: Turbine components such as blades, rings, discs and fasteners;Power Generation: Bolts, gas turbine components and other highly stressed components operating at elevated temperatures;Other: Combustion engine exhaust valves, die casting cores and inserts, high temperature springs | |
Corrosion properties | Excellent corrosion resistance | |
General machinability | Good machinability |