Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 25 % Show Material materials with Dehnung of 25 % | |
Elastizitätsmodul | 23.0 °C | 199 GPa Show Material materials with Elastizitätsmodul of 199 GPa | |
Härte, Brinell | 23.0 °C | 270 [-] Show Material materials with Härte, Brinell of 270 [-] | max. |
Poissonzahl | 23.0 °C | 0.32 [-] Show Material materials with Poissonzahl of 0.32 [-] | |
Schubmodule | 23.0 °C | 75 GPa Show Material materials with Schubmodule of 75 GPa | |
Streckgrenze Rp 0,2 | 23.0 °C | 550 MPa Show Material materials with Streckgrenze Rp 0,2 of 550 MPa | |
Zugfestigkeit | 23.0 °C | 750 MPa Show Material materials with Zugfestigkeit of 750 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.11E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.11E-5 1/K | for 20-100°C |
Spezifische Wärmekapazität | 23.0 °C | 425 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 425 J/(kg·K) | |
Wärmeleitfähigkeit | 23.0 °C | 14 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 14 W/(m·K) | for 20-300°C |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 8E-7 Ω·m Show Material materials with spezifischer Widerstand of 8E-7 Ω·m |
Magnetisch
Property | Temperature | Value |
---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 33 [-] Show Material materials with Relative magnetische Permeabilität of 33 [-] |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Chrom | 24 - 26 % Show Material materials with Chrom of 24 - 26 % | ||
Eisen | Balance | ||
Kohlenstoff | 0.03 % Show Material materials with Kohlenstoff of 0.03 % | max. | |
Kupfer | 0.5 - 1 % Show Material materials with Kupfer of 0.5 - 1 % | ||
Mangan | 1 % Show Material materials with Mangan of 1 % | max. | |
Molybdän | 3 - 4 % Show Material materials with Molybdän of 3 - 4 % | ||
Nickel | 6 - 8 % Show Material materials with Nickel of 6 - 8 % | ||
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % | max. | |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % | max. | |
Silizium | 1 % Show Material materials with Silizium of 1 % | max. | |
Stickstoff | 0.2 - 0.3 % Show Material materials with Stickstoff of 0.2 - 0.3 % | ||
Wolfram | 0.5 - 1 % Show Material materials with Wolfram of 0.5 - 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Offshore platforms, components for gas, oil and process cooling plants, instrumentation, wellhead and subsea wellhead fittings, desalination plants, seawater cooled heat exchangers, cargo heating systems, marine shafts (for boats etc) and high strength fasteners;Chemical processing: Equipment handling organic or dilute sulphuric acid, process solutions contaminated with chlorides, refinery equipment, desulphurising and distillation units, sewage plant components, fire extinguishing systems, general processing and mixing plant | |
Corrosion properties | Very good corrosion resistance |