Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 12 % Show Material materials with Dehnung of 12 % |
Härte, Brinell | 23.0 °C | 255 - 321 [-] Show Material materials with Härte, Brinell of 255 - 321 [-] |
Streckgrenze | 23.0 °C | 690 MPa Show Material materials with Streckgrenze of 690 MPa |
Zugfestigkeit | 23.0 °C | 880 - 1080 MPa Show Material materials with Zugfestigkeit of 880 - 1080 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Chrom | 16.5 % Show Material materials with Chrom of 16.5 % | ||
Eisen | Balance | ||
Kohlenstoff | 0.16 % Show Material materials with Kohlenstoff of 0.16 % | max. | |
Mangan | 0.3 % Show Material materials with Mangan of 0.3 % | ||
Nickel | 2.5 % Show Material materials with Nickel of 2.5 % | ||
Silizium | 0.25 % Show Material materials with Silizium of 0.25 % |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: High strength fasteners, bolts and shafts;Aerospace: Various aerospace components including high strength fasteners;Other: Compressor forms, dairies, machine tool industry, marine engineering, paper mills, plant engineering, starch mills and yeast factories | |
Corrosion properties | Excellent corrosion resistance |