Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 35 % Show Material materials with Dehnung of 35 % |
Härte, Brinell | 23.0 °C | 140 - 220 [-] Show Material materials with Härte, Brinell of 140 - 220 [-] |
Streckgrenze | 23.0 °C | 210 MPa Show Material materials with Streckgrenze of 210 MPa |
Zugfestigkeit | 23.0 °C | 540 MPa Show Material materials with Zugfestigkeit of 540 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Chrom | 18 % Show Material materials with Chrom of 18 % | ||
Eisen | Balance | ||
Kohlenstoff | 0.08 % Show Material materials with Kohlenstoff of 0.08 % | max. | |
Mangan | 1 % Show Material materials with Mangan of 1 % | ||
Molybdän | 1 % Show Material materials with Molybdän of 1 % | max. | |
Nickel | 9 % Show Material materials with Nickel of 9 % | ||
Niobium | 1.1 % Show Material materials with Niobium of 1.1 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace: Aerospace components and fasteners;Other: Breweries, cellulose, industry, dairies, fermentation industry, food processing, leather industry, machine tool industries, nitric acid plants, nuclear engineering, paper mills and production of explosives | |
Cold Forming | Good cold working characteristics | |
Corrosion properties | High corrosion resistance |