Mechanisch
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Chrom | 14 % Show Material materials with Chrom of 14 % | ||
Eisen | Balance | ||
Kohlenstoff | 0.07 % Show Material materials with Kohlenstoff of 0.07 % | max. | |
Kupfer | 1.6 % Show Material materials with Kupfer of 1.6 % | ||
Mangan | 1 % Show Material materials with Mangan of 1 % | max. | |
Molybdän | 1.6 % Show Material materials with Molybdän of 1.6 % | max. | |
Nickel | 5.4 % Show Material materials with Nickel of 5.4 % | ||
Silizium | 0.6 % Show Material materials with Silizium of 0.6 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace: Gas turbine blades, undercarriage components and fasteners | |
Corrosion properties | Good general corrosion resistance |