Allgemein
Property | Value | Related Standards | Shape |
---|---|---|---|
Dichte | 4.54 g/cm³ Show Material materials with Dichte of 4.54 g/cm³ | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Sheet, Plate, Bar, Billet |
4.54 g/cm³ Show Material materials with Dichte of 4.54 g/cm³ | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 |
Abmessung
Property | Temperature | Value | Shape | Related Standards | Comment |
---|---|---|---|---|---|
Breite | 400 mm Show Material materials with Breite of 400 mm | Sheet | |||
600 mm Show Material materials with Breite of 600 mm | Plate | ||||
1524 mm Show Material materials with Breite of 1524 mm | Sheet | ||||
1600 mm Show Material materials with Breite of 1600 mm | Plate | ||||
Dimensions | 15-65 mm diameter up to 6000 mm length °C | 7-14.5 mm diameter up to 3000 mm length | Bar | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142 | |
Durchmesser | 7 mm Show Material materials with Durchmesser of 7 mm | Bar | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142 | ||
115 mm Show Material materials with Durchmesser of 115 mm | Bar | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142 | |||
130 mm Show Material materials with Durchmesser of 130 mm | Billet | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556, MIL-F-82142 | |||
350 mm Show Material materials with Durchmesser of 350 mm | Billet | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556, MIL-F-82142 | |||
Länge | 1500 mm Show Material materials with Länge of 1500 mm | Sheet, Plate | |||
3000 mm Show Material materials with Länge of 3000 mm | Billet | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556, MIL-F-82142 | |||
4500 mm Show Material materials with Länge of 4500 mm | Billet | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556, MIL-F-82142 | |||
5000 mm Show Material materials with Länge of 5000 mm | Sheet | ||||
6000 mm Show Material materials with Länge of 6000 mm | Bar | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142 | max | ||
6500 mm Show Material materials with Länge of 6500 mm | Plate |
valueMetaData
Property | Value |
---|
Mechanisch
Property | Value | Related Standards | Shape |
---|---|---|---|
Dehnung | 13.0 % Show Material materials with Dehnung of 13.0 % | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Sheet, Plate, Bar, Billet |
Elastizitätsmodul | 114 GPa Show Material materials with Elastizitätsmodul of 114 GPa | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 | |
118.0 GPa Show Material materials with Elastizitätsmodul of 118.0 GPa | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Sheet, Plate, Bar, Billet | |
Härte, Brinell | 318.0 Show Material materials with Härte, Brinell of 318.0 | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Sheet, Plate, Bar, Billet |
Härte, Rockwell C | 34.0 Show Material materials with Härte, Rockwell C of 34.0 | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Sheet, Plate, Bar, Billet |
Härte, Vickers | 333.0 Show Material materials with Härte, Vickers of 333.0 | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Sheet, Plate, Bar, Billet |
Poissonzahl | 0.325 [-] Show Material materials with Poissonzahl of 0.325 [-] | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Sheet, Plate, Bar, Billet |
Schubmodule | 44.5 GPa Show Material materials with Schubmodule of 44.5 GPa | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Sheet, Plate, Bar, Billet |
Streckgrenze | 827.0 MPa Show Material materials with Streckgrenze of 827.0 MPa | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 | |
1050.0 MPa Show Material materials with Streckgrenze of 1050.0 MPa | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Sheet, Plate, Bar, Billet | |
Zugfestigkeit | 996.0 MPa Show Material materials with Zugfestigkeit of 996.0 MPa | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 | |
1110.0 MPa Show Material materials with Zugfestigkeit of 1110.0 MPa | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Sheet, Plate, Bar, Billet |
Thermisch
Property | Temperature | Value | Related Standards | Shape |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 0.0000077 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.0000077 1/K | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 | |
Schmelzpunkt | 1704.0 °C Show Material materials with Schmelzpunkt of 1704.0 °C | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 | ||
1705.0 °C Show Material materials with Schmelzpunkt of 1705.0 °C | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Sheet, Plate, Bar, Billet | ||
Spezifische Wärmekapazität | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 | ||
Wärmeleitfähigkeit | 7 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 7 W/(m·K) | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Sheet, Plate, Bar, Billet | |
7.7 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 7.7 W/(m·K) | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 |
Elektrisch
Property | Value | Related Standards |
---|---|---|
spezifischer Widerstand | 1.85e-06 Ω·m Show Material materials with spezifischer Widerstand of 1.85e-06 Ω·m | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 5.5 - 6.5 % Show Material materials with Aluminium of 5.5 - 6.5 % | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142, AMS 4975, AMS 4919 | Sheet, Plate, Bar, Billet |
Eisen | 0.25 Show Material materials with Eisen of 0.25 | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142, AMS 4975, AMS 4919 | Sheet, Plate, Bar, Billet |
Kohlenstoff | 0.05 Show Material materials with Kohlenstoff of 0.05 | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Sheet, Plate, Bar, Billet |
0.08 Show Material materials with Kohlenstoff of 0.08 | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 | ||
Molybdän | 1.75 - 2.25 % Show Material materials with Molybdän of 1.75 - 2.25 % | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 | |
1.8 - 2.2 % Show Material materials with Molybdän of 1.8 - 2.2 % | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Sheet, Plate, Bar, Billet | |
Sauerstoff | 0.12 Show Material materials with Sauerstoff of 0.12 | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142, AMS 4975, AMS 4919 | Bar, Billet |
0.15 Show Material materials with Sauerstoff of 0.15 | Sheet, Plate | ||
Silizium | 0.06 - 0.1 % Show Material materials with Silizium of 0.06 - 0.1 % | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Sheet, Plate, Bar, Billet |
0.1 % Show Material materials with Silizium of 0.1 % | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 | ||
Stickstoff | 0.05 Show Material materials with Stickstoff of 0.05 | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142, AMS 4975, AMS 4919 | Sheet, Plate, Bar, Billet |
Wasserstoff | 0.01 Show Material materials with Wasserstoff of 0.01 | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 | |
0.015 Show Material materials with Wasserstoff of 0.015 | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Sheet, Plate, Bar, Billet | |
Zinn | 1.75 - 2.25 % Show Material materials with Zinn of 1.75 - 2.25 % | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 | |
1.8 - 2.2 % Show Material materials with Zinn of 1.8 - 2.2 % | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Sheet, Plate, Bar, Billet | |
Zirkonium | 3.5 - 4.5 % Show Material materials with Zirkonium of 3.5 - 4.5 % | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 | |
3.6 - 4.4 % Show Material materials with Zirkonium of 3.6 - 4.4 % | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Sheet, Plate, Bar, Billet |