Grades provided by the supplier

Grade Shape Equivalent Materials Standard / Norm 

Alloy 188

Strip, Sheet, Wire

Alloy 188, UNS R30188

AMS 5608, AMS 5772, AMS 5609

Alloy 20

Plate, Pipe, Bar, Sheet, Tube, Wire

Alloy 20, UNS N08020

ASTM B463, ASME SB463

Alloy 22

Fitting, Plate, Pipe, Bar, Sheet, Tube

Alloy 22, UNS N06022

ASTM B575, ASME SB575

Alloy 36

Plate, Bar, Wire

Alloy 36, UNS K93603

ASTM B753, ASTM F-1684, MIL-I-23011

Alloy 400

Fitting, Plate, Pipe, Bar, Sheet, Tube, Strip, Wire

Alloy 400, UNS N04400

ASTM B127, ASME SB127, AMS 4544, QQ-N-281

Alloy 41

Strip, Sheet, Wire

Alloy 41, UNS N07041

AMS 5545, AMS 5712, AMS 5800

Alloy 600

Fitting, Plate, Pipe, Bar, Sheet, Tube, Strip, Wire

Alloy 600, UNS N06600

STM B-168, ASME SB168, AMS 5540, MIL-N-23228, MIL-T-23227

Alloy 601

Plate, Pipe, Sheet, Tube, Strip

Alloy 601, UNS N06601

ASTM B168, AMS 5870

Alloy 617

Wire

Alloy 617, UNS N06617

AMS 5888, AMS 5889, ASME SB168, ASME 166B, ASME 472, AMS 5887, SFA 5.11 (ENiCrCoMo-1), A 5.11 (ENiCrCoMo-1), SFA 5.14 (ERNiCrCoMo-1), A 5.14 (ERNiCrCoMo-1), ASME SB167, ASME SB564

Alloy 625

Plate, Bar, Sheet, Strip, Tube, Wire

Alloy 625, UNS N06625

ASTM B443, ASME SB443, AMS 5599