Allgemein
Property | Value | Shape |
---|---|---|
Dichte | 4.65 g/cm³ Show Material materials with Dichte of 4.65 g/cm³ | Bar, Billet |
Abmessung
Property | Temperature | Value | Shape | Comment |
---|---|---|---|---|
Dimensions | 15-65 mm diameter up to 6000 mm length °C | 7-14.5 mm diameter up to 3000 mm length | Bar | |
Durchmesser | 7 mm Show Material materials with Durchmesser of 7 mm | Bar | ||
115 mm Show Material materials with Durchmesser of 115 mm | Bar | |||
130 mm Show Material materials with Durchmesser of 130 mm | Billet | |||
350 mm Show Material materials with Durchmesser of 350 mm | Billet | |||
Länge | 3000 mm Show Material materials with Länge of 3000 mm | Billet | ||
4500 mm Show Material materials with Länge of 4500 mm | Billet | |||
6000 mm Show Material materials with Länge of 6000 mm | Bar | max |
Mechanisch
Property | Value | Shape |
---|---|---|
Dehnung | 9.0 % Show Material materials with Dehnung of 9.0 % | Bar, Billet |
Elastizitätsmodul | 110.0 Show Material materials with Elastizitätsmodul of 110.0 | Bar, Billet |
Härte, Brinell | 304.0 Show Material materials with Härte, Brinell of 304.0 | Bar, Billet |
Härte, Rockwell C | 32.0 [-] Show Material materials with Härte, Rockwell C of 32.0 [-] | Bar, Billet |
Härte, Vickers | 318.0 Show Material materials with Härte, Vickers of 318.0 | Bar, Billet |
Schubmodule | 41.0 GPa Show Material materials with Schubmodule of 41.0 GPa | Bar, Billet |
Streckgrenze | 900.0 MPa Show Material materials with Streckgrenze of 900.0 MPa | Bar, Billet |
Zugfestigkeit | 970.0 MPa Show Material materials with Zugfestigkeit of 970.0 MPa | Bar, Billet |
Thermisch
Property | Value | Shape | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 7.099999999999997e-06 - 9.699999999999999e-06 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 7.099999999999997e-06 - 9.699999999999999e-06 1/K | Typical for Titanium Beta Alloy | |
Schmelzpunkt | 1550.0 - 1815.0 °C Show Material materials with Schmelzpunkt of 1550.0 - 1815.0 °C | Typical for Titanium Beta Alloy | |
Spezifische Wärmekapazität | 490.0 - 580.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 490.0 - 580.0 J/(kg·K) | Typical for Titanium Beta Alloy | |
Wärmeleitfähigkeit | 7.8 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 7.8 W/(m·K) | Bar, Billet |
Chemical properties
Property | Value | Shape |
---|---|---|
Aluminium | 2.6 - 3.4 % Show Material materials with Aluminium of 2.6 - 3.4 % | Bar, Billet |
Eisen | 1.6 - 2.2 % Show Material materials with Eisen of 1.6 - 2.2 % | Bar, Billet |
Kohlenstoff | 0.05 % Show Material materials with Kohlenstoff of 0.05 % | Bar, Billet |
Sauerstoff | 0.13 Show Material materials with Sauerstoff of 0.13 | Bar, Billet |
Stickstoff | 0.05 Show Material materials with Stickstoff of 0.05 | Bar, Billet |
Vanadium | 9.0 - 11.0 % Show Material materials with Vanadium of 9.0 - 11.0 % | Bar, Billet |
Wasserstoff | 0.015 Show Material materials with Wasserstoff of 0.015 | Bar, Billet |