Grades provided by the supplier

Grade Shape Equivalent Materials Standard / Norm 

13-8 PH

Bar, Ring, Forging, Disc, Sheet, Plate, Extrusion, Billet, Ingot

13-8 PH, UNS S13800

ASTM A 693, ASTM A 705, ASTM A 564, AMS 5840, AMS 5629

15-5 PH

Bar, Ring, Forging, Disc, Sheet, Plate, Extrusion, Billet, Ingot

15-5 PH, UNS S15500

ASTM A 698, ASME SA 693, ASTM A 705, ASTM A 564, AMS 5862, ASME SA 564, AMS 5659

AerMet 100

Bar, Ring, Forging, Disc, Sheet, Plate, Extrusion, Billet, Ingot

UNS K92580

MIL STD 2154 CL A, MIL STD 2154 TYPE 1 CL A, AMS 6532, M L HDBK-5, MMS 217, MIL HDBK 5

AISI 4330

Bar, Ring, Forging, Disc, Sheet, Plate, Extrusion, Billet, Ingot

AISI 4330

AMS 6415, AMS 6359

AISI 4330M

Bar, Ring, Forging, Disc, Sheet, Plate, Extrusion, Billet, Ingot

AISI 4330M

AMS 6427, MIL-S-8699, AMS 2300, AMS 6411

Alloy 200

Bar, Ring, Forging, Disc, Sheet, Plate, Extrusion, Billet, Ingot

UNS N02200, DIN 2.4060, DIN 2.4066

DIN 17750, ASTM B161, BS 3074, BS 3072, DIN 17752, ASTM B160, ASTM B366, ASTM B163, ASTM B622, DIN 17740, ASTM B162, BS 3076, ASTM B564

Alloy 201

Bar, Ring, Forging, Disc, Sheet, Plate, Extrusion, Billet, Ingot

UNS N02201, DIN 2.4061, DIN 2.4068

DIN 17750, B366, BS 3072, DIN 17752, DIN 17754, ASTM B160, AMS 5553, NA 12, ASTM B162, BS 3076, ASTM B564

Custom 465

Bar, Ring, Forging, Disc, Sheet, Plate, Extrusion, Billet, Ingot

UNS S46500

AMS 5936, MMPDS-01, ASTM A693, ASTM A564, ASTM F899

DIN 3.1255

Bar, Ring, Forging, Disc, Sheet, Plate, Extrusion, Billet, Ingot

DIN 3.1255, UNS A92014, EN AW-2014, AA 2014

ASTM B241, SAE J454, ASTM B209, ASTM BB241, ASTM B247, QQ A-225/4, QQ A-250/4, QQ A-200/2, QQ A-367, ASTM B211, ASTM B210, ASTM B221, MIL T-15089

DIN 3.1924

Bar, Ring, Forging, Disc, Sheet, Plate, Extrusion, Billet, Ingot

DIN 3.1924, EN 2123, EN 3553, EN AW-2618, AA 2618

AIR 9048.170, UNI 9002/6, SO7-1103, AIR 9048.640 T851, DTD 5014, BAEM 1103, CM001-1 T6, DTD 731B, GB-D19S, CCT LA 767, AIR 9048.150, AIR 9048.640 T351, BAEM 1101, DTD 717A, ASN-A-3355, CM001-3 H28, DTD 5070B, Hiduminium 58, AIRBUS-ABM1-1006, BS Pre-1980 H16, L-3171, AIR 9051A, AIR 9048.640, MM 0531, A-U2GN, MSRR 8016, DTD 5084A, MSRR 8018, DTD 745A, ASN-A-3357