Allgemein
Property | Value | Related Standards | Shape |
---|---|---|---|
Dichte | 4.51 g/cm³ Show Material materials with Dichte of 4.51 g/cm³ | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube |
Abmessung
Property | Value | Related Standards | Shape |
---|---|---|---|
Breite | 400 mm Show Material materials with Breite of 400 mm | ASTM B-265, DIN 17860 | Sheet |
600 mm Show Material materials with Breite of 600 mm | ASTM B-265, DIN 17860 | Plate | |
1524 mm Show Material materials with Breite of 1524 mm | ASTM B-265, DIN 17860 | Sheet | |
1600 mm Show Material materials with Breite of 1600 mm | ASTM B-265, DIN 17860 | Plate | |
Durchmesser | 5 mm Show Material materials with Durchmesser of 5 mm | ASTM B-265, DIN 17860 | Tube |
12.7 mm Show Material materials with Durchmesser of 12.7 mm | ASTM B-265, DIN 17860 | Tube | |
25.4 mm Show Material materials with Durchmesser of 25.4 mm | ASTM B-265, DIN 17860 | Billet | |
38.1 mm Show Material materials with Durchmesser of 38.1 mm | ASTM B-265, DIN 17860 | Tube | |
125 mm Show Material materials with Durchmesser of 125 mm | ASTM B-265, DIN 17860 | Billet | |
130 mm Show Material materials with Durchmesser of 130 mm | ASTM B-265, DIN 17860 | Tube | |
Länge | 1000 mm Show Material materials with Länge of 1000 mm | ASTM B-265, DIN 17860 | Tube |
1500 mm Show Material materials with Länge of 1500 mm | ASTM B-265, DIN 17860 | Sheet, Plate | |
5000 mm Show Material materials with Länge of 5000 mm | ASTM B-265, DIN 17860 | Sheet, Tube | |
6500 mm Show Material materials with Länge of 6500 mm | ASTM B-265, DIN 17860 | Plate | |
20000 mm Show Material materials with Länge of 20000 mm | ASTM B-265, DIN 17860 | Tube | |
Wall thickness | 0.4 - 1.65 mm Show Material materials with Wall thickness of 0.4 - 1.65 mm | ASTM B-265, DIN 17860 | Tube |
0.5 - 9.0 mm Show Material materials with Wall thickness of 0.5 - 9.0 mm | ASTM B-265, DIN 17860 | Tube | |
2.5 - 21.0 mm Show Material materials with Wall thickness of 2.5 - 21.0 mm | ASTM B-265, DIN 17860 | Billet |
valueMetaData
Property | Value |
---|
Mechanisch
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Dehnung | 22.0 % Show Material materials with Dehnung of 22.0 % | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube | |
Elastizitätsmodul | 105.0 GPa Show Material materials with Elastizitätsmodul of 105.0 GPa | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube | |
Härte, Brinell | 120.0 Show Material materials with Härte, Brinell of 120.0 | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube | |
Poissonzahl | 0.361 [-] Show Material materials with Poissonzahl of 0.361 [-] | Typical for Pure Titanium | ||
Schubmodule | 46.0 GPa Show Material materials with Schubmodule of 46.0 GPa | Typical for Pure Titanium | ||
Streckgrenze | 170.0 MPa Show Material materials with Streckgrenze of 170.0 MPa | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube | |
Zugfestigkeit | 240.0 MPa Show Material materials with Zugfestigkeit of 240.0 MPa | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube |
Thermisch
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Pure Titanium | ||
Schmelzpunkt | 1670.0 °C Show Material materials with Schmelzpunkt of 1670.0 °C | Typical for Pure Titanium | ||
Spezifische Wärmekapazität | 520 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 520 J/(kg·K) | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube | |
Wärmeleitfähigkeit | 21 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 21 W/(m·K) | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Eisen | 0.2 Show Material materials with Eisen of 0.2 | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube |
Kohlenstoff | 0.08 Show Material materials with Kohlenstoff of 0.08 | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube |
Sauerstoff | 0.18 Show Material materials with Sauerstoff of 0.18 | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube |
Stickstoff | 0.03 Show Material materials with Stickstoff of 0.03 | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube |
Wasserstoff | 0.015 Show Material materials with Wasserstoff of 0.015 | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube |