Allgemein
Property | Value |
---|---|
Dichte | 1.18 - 1.25 g/cm³ Show Material materials with Dichte of 1.18 - 1.25 g/cm³ |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 5.0 - 25.0 % Show Material materials with Dehnung of 5.0 - 25.0 % | |
Elastizitätsmodul | 2.6 - 4.0 GPa Show Material materials with Elastizitätsmodul of 2.6 - 4.0 GPa | |
Schlagfestigkeit, Charpy gekerbt | 10.0 - 35.0 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 10.0 - 35.0 kJ/m² | |
Schlagzähigkeit, Charpy ungekerbt | 65 kJ/m² Show Material materials with Schlagzähigkeit, Charpy ungekerbt of 65 kJ/m² | |
Zugfestigkeit | 55.0 - 75.0 MPa Show Material materials with Zugfestigkeit of 55.0 - 75.0 MPa | at 5-25% strain |
Thermisch
Property | Value |
---|---|
Koeffizient der thermischen Ausdehnung | 3e-05 - 0.00012 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 3e-05 - 0.00012 1/K |
Schmelzpunkt | 220.0 - 225.0 °C Show Material materials with Schmelzpunkt of 220.0 - 225.0 °C |
Entflammbarkeit | UL 94 HB |
Elektrisch
Property | Value |
---|---|
Dielektrizitätskonstante | 3.5 [-] Show Material materials with Dielektrizitätskonstante of 3.5 [-] |
14 [-] Show Material materials with Dielektrizitätskonstante of 14 [-] | |
spezifischer Widerstand | 1000000000.0 - 100000000000000.0 Ω·m Show Material materials with spezifischer Widerstand of 1000000000.0 - 100000000000000.0 Ω·m |
Optisch
Property | Value |
---|---|
Transparenz | no |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive plugs and seals, counter wheel sensors, plug housings, grip handles, automotive mirror housings, wheels of moutain bikes | |
Fillers | 15% Glass Fiber | |
Other | You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application: Polymer Advanced Search | |
Processing methods | Injection molding, blow molding, extrusion |