Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.75 - 1.5 % Show Material materials with Aluminium of 0.75 - 1.5 % | |
Chrom | 16 - 18 % Show Material materials with Chrom of 16 - 18 % | |
Eisen | 70.58 - 76.75 % Show Material materials with Eisen of 70.58 - 76.75 % | balance |
Kohlenstoff | 0.09 % Show Material materials with Kohlenstoff of 0.09 % | |
Mangan | 1 % Show Material materials with Mangan of 1 % | |
Nickel | 6.5 - 7.75 % Show Material materials with Nickel of 6.5 - 7.75 % | |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % | |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % | |
Silizium | 1 % Show Material materials with Silizium of 1 % |