Property | Value | Comment |
---|---|---|
Dichte | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Value | Comment |
---|---|---|
Elastizitätsmodul | 190.0 - 210.0 GPa Show Material materials with Elastizitätsmodul of 190.0 - 210.0 GPa | Typical for Steel |
Poissonzahl | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Chemical properties
Property | Value | Related Standards |
---|---|---|
Bor | 0.0005 % Show Material materials with Bor of 0.0005 % | SAE J407 |
Chrom | 0.25 - 0.55 % Show Material materials with Chrom of 0.25 - 0.55 % | SAE J407 |
Eisen | 99.9949 - 99.9989 % Show Material materials with Eisen of 99.9949 - 99.9989 % | SAE J407 |
Kohlenstoff | 0.12 - 0.18 % Show Material materials with Kohlenstoff of 0.12 - 0.18 % | SAE J407 |
Kupfer | 0.35 Show Material materials with Kupfer of 0.35 | SAE J407 |
Mangan | 0.7 - 1.05 % Show Material materials with Mangan of 0.7 - 1.05 % | SAE J407 |
Molybdän | 0.08 - 0.15 % Show Material materials with Molybdän of 0.08 - 0.15 % | SAE J407 |
Nickel | 0.25 - 0.65 % Show Material materials with Nickel of 0.25 - 0.65 % | SAE J407 |
Phosphor | 0.035 Show Material materials with Phosphor of 0.035 | SAE J407 |
Schwefel | 0.035 - 0.05 % Show Material materials with Schwefel of 0.035 - 0.05 % | SAE J407 |
Silizium | 0.15 - 0.35 % Show Material materials with Silizium of 0.15 - 0.35 % | SAE J407 |