Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 5 % Show Material materials with Aluminium of 5 % |
Bor | 0.015 % Show Material materials with Bor of 0.015 % |
Chrom | 9 % Show Material materials with Chrom of 9 % |
Eisen | 60.28 - 100 % Show Material materials with Eisen of 60.28 - 100 % |
Kobalt | 10 % Show Material materials with Kobalt of 10 % |
Kohlenstoff | 0.15 % Show Material materials with Kohlenstoff of 0.15 % |
Niobium | 1 % Show Material materials with Niobium of 1 % |
Titan | 2 % Show Material materials with Titan of 2 % |
Wolfram | 12.5 % Show Material materials with Wolfram of 12.5 % |
Zirkonium | 0.05 % Show Material materials with Zirkonium of 0.05 % |