Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 1.17 % Show Material materials with Aluminium of 1.17 % |
Chrom | 15 % Show Material materials with Chrom of 15 % |
Eisen | 69.59 - 76.75 % Show Material materials with Eisen of 69.59 - 76.75 % |
Kohlenstoff | 0.07 % Show Material materials with Kohlenstoff of 0.07 % |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % |
Molybdän | 2.2 % Show Material materials with Molybdän of 2.2 % |
Nickel | 7 % Show Material materials with Nickel of 7 % |
Silizium | 0.3 % Show Material materials with Silizium of 0.3 % |