Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.72 g/cm³ Show Material materials with Dichte of 7.72 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 20 % Show Material materials with Dehnung of 20 % | |
Elastizitätsmodul | 23.0 °C | 195 GPa Show Material materials with Elastizitätsmodul of 195 GPa | Typical for Austenitic Stainless Steel |
Flächenreduzierung | 20.0 °C | 15 % Show Material materials with Flächenreduzierung of 15 % | |
650.0 °C | 48 % Show Material materials with Flächenreduzierung of 48 % | ||
760.0 °C | 14 % Show Material materials with Flächenreduzierung of 14 % | ||
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Austenitic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Austenitic Stainless Steel |
Streckgrenze | 20.0 °C | 520 MPa Show Material materials with Streckgrenze of 520 MPa | |
650.0 °C | 260 MPa Show Material materials with Streckgrenze of 260 MPa | ||
760.0 °C | 210 MPa Show Material materials with Streckgrenze of 210 MPa | ||
Zugfestigkeit | 20.0 °C | 1030 MPa Show Material materials with Zugfestigkeit of 1030 MPa | |
650.0 °C | 500 MPa Show Material materials with Zugfestigkeit of 500 MPa | ||
760.0 °C | 340 MPa Show Material materials with Zugfestigkeit of 340 MPa | ||
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 760.0 °C | 1.88E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.88E-5 1/K | The mentioned value is between 20°C and the mentioned temperature |
Schmelzpunkt | 1230 - 1480 °C Show Material materials with Schmelzpunkt of 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Spezifische Wärmekapazität | 23.0 °C | 440 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 440 J/(kg·K) | Typical for Austenitic Stainless Steel |
Wärmeleitfähigkeit | 23.0 °C | 11 - 21 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 11 - 21 W/(m·K) | Typical for Austenitic Stainless Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 8.5E-7 Ω·m Show Material materials with spezifischer Widerstand of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 20 - 22 % Show Material materials with Chrom of 20 - 22 % | |
Eisen | 67.22 - 71.82 % Show Material materials with Eisen of 67.22 - 71.82 % | Balance |
Kohlenstoff | 0.65 - 0.75 % Show Material materials with Kohlenstoff of 0.65 - 0.75 % | |
Mangan | 5.5 - 7 % Show Material materials with Mangan of 5.5 - 7 % | |
Nickel | 1.4 - 1.9 % Show Material materials with Nickel of 1.4 - 1.9 % | |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % | |
Schwefel | 0.025 - 0.065 % Show Material materials with Schwefel of 0.025 - 0.065 % | |
Silizium | 0.45 - 0.85 % Show Material materials with Silizium of 0.45 - 0.85 % | |
Stickstoff | 0.18 - 0.28 % Show Material materials with Stickstoff of 0.18 - 0.28 % |