Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.6 - 7.8 g/cm³ Show Material materials with Dichte of 7.6 - 7.8 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 195 GPa Show Material materials with Elastizitätsmodul of 195 GPa | Typical for Austenitic Stainless Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Austenitic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Austenitic Stainless Steel |
Streckgrenze | 23.0 °C | 553 - 700 MPa Show Material materials with Streckgrenze of 553 - 700 MPa | |
Zugfestigkeit | 23.0 °C | 862 - 1155 MPa Show Material materials with Zugfestigkeit of 862 - 1155 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 200.0 °C | 1.44E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.44E-5 1/K | The mentioned values are between 20°C and the mentioned temperature |
700.0 °C | 1.75E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.75E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
1000.0 °C | 1.85E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.85E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
Schmelzpunkt | 1230 - 1480 °C Show Material materials with Schmelzpunkt of 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Spezifische Wärmekapazität | 23.0 °C | 440 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 440 J/(kg·K) | Typical for Austenitic Stainless Steel |
Wärmeleitfähigkeit | 23.0 °C | 11 - 21 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 11 - 21 W/(m·K) | Typical for Austenitic Stainless Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 8.5E-7 Ω·m Show Material materials with spezifischer Widerstand of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 19.5 - 21.5 % Show Material materials with Chrom of 19.5 - 21.5 % | |
Eisen | 65 - 71.55 % Show Material materials with Eisen of 65 - 71.55 % | Balance |
Kohlenstoff | 0.5 - 0.6 % Show Material materials with Kohlenstoff of 0.5 - 0.6 % | |
Mangan | 7 - 10 % Show Material materials with Mangan of 7 - 10 % | |
Nickel | 1.5 - 2.75 % Show Material materials with Nickel of 1.5 - 2.75 % | |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % | |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % | |
Silizium | 0.25 % Show Material materials with Silizium of 0.25 % | |
Stickstoff | 0.2 - 0.4 % Show Material materials with Stickstoff of 0.2 - 0.4 % |