Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 20.0 °C | 61 % Show Material materials with Flächenreduzierung of 61 % | |
650.0 °C | 60 % Show Material materials with Flächenreduzierung of 60 % | ||
760.0 °C | 60 % Show Material materials with Flächenreduzierung of 60 % | ||
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 20.0 °C | 480 MPa Show Material materials with Streckgrenze of 480 MPa | |
650.0 °C | 220 MPa Show Material materials with Streckgrenze of 220 MPa | ||
760.0 °C | 190 MPa Show Material materials with Streckgrenze of 190 MPa | ||
Zugfestigkeit | 20.0 °C | 880 MPa Show Material materials with Zugfestigkeit of 880 MPa | |
650.0 °C | 490 MPa Show Material materials with Zugfestigkeit of 490 MPa | ||
760.0 °C | 320 MPa Show Material materials with Zugfestigkeit of 320 MPa | ||
Chemical properties
Property | Value |
---|---|
Chrom | 21 % Show Material materials with Chrom of 21 % |
Eisen | 66.2 - 100 % Show Material materials with Eisen of 66.2 - 100 % |
Kohlenstoff | 0.2 % Show Material materials with Kohlenstoff of 0.2 % |
Mangan | 6.5 % Show Material materials with Mangan of 6.5 % |
Nickel | 5.5 % Show Material materials with Nickel of 5.5 % |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % |
Stickstoff | 0.2 % Show Material materials with Stickstoff of 0.2 % |