Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 20 % Show Material materials with Dehnung A5 of 20 % | |
Elastizitätsmodul | 23.0 °C | 205 GPa Show Material materials with Elastizitätsmodul of 205 GPa | |
Flächenreduzierung | 23.0 °C | 30 - 33 % Show Material materials with Flächenreduzierung of 30 - 33 % | |
Härte, Rockwell C | 23.0 °C | 25 [-] Show Material materials with Härte, Rockwell C of 25 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Austenitic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Austenitic Stainless Steel |
Streckgrenze | 23.0 °C | 550 - 634 MPa Show Material materials with Streckgrenze of 550 - 634 MPa | |
Zugfestigkeit | 23.0 °C | 850 - 1100 MPa Show Material materials with Zugfestigkeit of 850 - 1100 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 1.65E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.65E-5 1/K | The mentioned values are between 20°C and the mentioned temperature |
300.0 °C | 1.7E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
500.0 °C | 1.73E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.73E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
700.0 °C | 1.74E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.74E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
Schmelzpunkt | 1230 - 1480 °C Show Material materials with Schmelzpunkt of 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Spezifische Wärmekapazität | 23.0 °C | 500 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 500 J/(kg·K) | |
Wärmeleitfähigkeit | 23.0 °C | 14.5 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 14.5 W/(m·K) |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 8.5E-7 Ω·m Show Material materials with spezifischer Widerstand of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 22 - 24 % Show Material materials with Chrom of 22 - 24 % |
Eisen | 64.59 - 100 % Show Material materials with Eisen of 64.59 - 100 % |
Kohlenstoff | 0.28 - 0.38 % Show Material materials with Kohlenstoff of 0.28 - 0.38 % |
Mangan | 1.5 - 3.5 % Show Material materials with Mangan of 1.5 - 3.5 % |
Molybdän | 0.5 % Show Material materials with Molybdän of 0.5 % |
Nickel | 7 - 9 % Show Material materials with Nickel of 7 - 9 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 0.5 - 1 % Show Material materials with Silizium of 0.5 - 1 % |
Stickstoff | 0.25 - 0.35 % Show Material materials with Stickstoff of 0.25 - 0.35 % |
Wolfram | 0.5 % Show Material materials with Wolfram of 0.5 % |