Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.9 g/cm³ Show Material materials with Dichte of 7.9 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 17 % Show Material materials with Dehnung A5 of 17 % | |
Elastizitätsmodul | 23.0 °C | 194 GPa Show Material materials with Elastizitätsmodul of 194 GPa | |
Härte, Rockwell C | 23.0 °C | 24 - 30 [-] Show Material materials with Härte, Rockwell C of 24 - 30 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Austenitic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Austenitic Stainless Steel |
Streckgrenze | 23.0 °C | 900 - 1000 MPa Show Material materials with Streckgrenze of 900 - 1000 MPa | |
Zugfestigkeit | 23.0 °C | 1000 - 1150 MPa Show Material materials with Zugfestigkeit of 1000 - 1150 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 200.0 °C | 1.73E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.73E-5 1/K | The mentioned values are between 20°C and the mentioned temperature |
600.0 °C | 1.78E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.78E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
Schmelzpunkt | 1230 - 1480 °C Show Material materials with Schmelzpunkt of 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Spezifische Wärmekapazität | 23.0 °C | 500 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 500 J/(kg·K) | |
Wärmeleitfähigkeit | 23.0 °C | 16.3 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 16.3 W/(m·K) |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 8.5E-7 Ω·m Show Material materials with spezifischer Widerstand of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 17 - 19 % Show Material materials with Chrom of 17 - 19 % | |
Eisen | 63.9 - 72 % Show Material materials with Eisen of 63.9 - 72 % | Balance |
Kohlenstoff | 0.1 % Show Material materials with Kohlenstoff of 0.1 % | |
Kupfer | 3 - 4 % Show Material materials with Kupfer of 3 - 4 % | |
Mangan | 2 % Show Material materials with Mangan of 2 % | |
Nickel | 8 - 10 % Show Material materials with Nickel of 8 - 10 % | |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % | |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % | |
Silizium | 1 % Show Material materials with Silizium of 1 % |