Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.7 - 7.8 g/cm³ Show Material materials with Dichte of 7.7 - 7.8 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 7 - 24 % Show Material materials with Dehnung A5 of 7 - 24 % | |
Elastizitätsmodul | 23.0 °C | 201 GPa Show Material materials with Elastizitätsmodul of 201 GPa | |
Flächenreduzierung | 23.0 °C | 4 - 20 % Show Material materials with Flächenreduzierung of 4 - 20 % | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Austenitic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Austenitic Stainless Steel |
Streckgrenze | 23.0 °C | 415 - 763 MPa Show Material materials with Streckgrenze of 415 - 763 MPa | |
Zugfestigkeit | 23.0 °C | 795 - 865 MPa Show Material materials with Zugfestigkeit of 795 - 865 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 200.0 °C | 1.48E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.48E-5 1/K | The mentioned values are between 20°C and the mentioned temperature |
600.0 °C | 1.58E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.58E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
1000.0 °C | 1.73E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.73E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
1300.0 °C | 1.85E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.85E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
Schmelzpunkt | 1230 - 1480 °C Show Material materials with Schmelzpunkt of 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Spezifische Wärmekapazität | 23.0 °C | 440 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 440 J/(kg·K) | Typical for Austenitic Stainless Steel |
Wärmeleitfähigkeit | 23.0 °C | 11 - 21 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 11 - 21 W/(m·K) | Typical for Austenitic Stainless Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 8.5E-7 Ω·m Show Material materials with spezifischer Widerstand of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 20 - 22 % Show Material materials with Chrom of 20 - 22 % | |
Eisen | 62.55 - 67.5 % Show Material materials with Eisen of 62.55 - 67.5 % | Balance |
Kohlenstoff | 0.15 - 0.25 % Show Material materials with Kohlenstoff of 0.15 - 0.25 % | |
Mangan | 1 - 1.5 % Show Material materials with Mangan of 1 - 1.5 % | |
Nickel | 10.5 - 12.5 % Show Material materials with Nickel of 10.5 - 12.5 % | |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % | |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % | |
Silizium | 2 - 3 % Show Material materials with Silizium of 2 - 3 % | |
Stickstoff | 0.15 - 0.25 % Show Material materials with Stickstoff of 0.15 - 0.25 % |