Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.91 g/cm³ Show Material materials with Dichte of 7.91 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 20.0 °C | 49 % Show Material materials with Flächenreduzierung of 49 % | |
650.0 °C | 14 % Show Material materials with Flächenreduzierung of 14 % | ||
760.0 °C | 23 % Show Material materials with Flächenreduzierung of 23 % | ||
Härte, Brinell | 760.0 °C | 120 [-] Show Material materials with Härte, Brinell of 120 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 20.0 °C | 700 MPa Show Material materials with Streckgrenze of 700 MPa | |
650.0 °C | 610 MPa Show Material materials with Streckgrenze of 610 MPa | ||
760.0 °C | 340 MPa Show Material materials with Streckgrenze of 340 MPa | ||
Zugfestigkeit | 20.0 °C | 1030 MPa Show Material materials with Zugfestigkeit of 1030 MPa | |
650.0 °C | 720 MPa Show Material materials with Zugfestigkeit of 720 MPa | ||
760.0 °C | 440 MPa Show Material materials with Zugfestigkeit of 440 MPa | ||
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 760.0 °C | 1.5E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.5E-5 1/K | The mentioned value is between 20°C and the mentioned temperature |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.35 % Show Material materials with Aluminium of 0.35 % |
Bor | 0.001 - 0.01 % Show Material materials with Bor of 0.001 - 0.01 % |
Chrom | 13.5 - 16 % Show Material materials with Chrom of 13.5 - 16 % |
Eisen | 49.14 - 59.5 % Show Material materials with Eisen of 49.14 - 59.5 % |
Kohlenstoff | 0.08 % Show Material materials with Kohlenstoff of 0.08 % |
Mangan | 2 % Show Material materials with Mangan of 2 % |
Molybdän | 1 - 1.5 % Show Material materials with Molybdän of 1 - 1.5 % |
Nickel | 24 - 27 % Show Material materials with Nickel of 24 - 27 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Titan | 1.9 % Show Material materials with Titan of 1.9 % |
Vanadium | 0.1 - 0.5 % Show Material materials with Vanadium of 0.1 - 0.5 % |