Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.9 - 8 g/cm³ Show Material materials with Dichte of 7.9 - 8 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A5 | 20.0 °C | 25 - 35 % Show Material materials with Dehnung A5 of 25 - 35 % |
Elastizitätsmodul | 20.0 °C | 208 GPa Show Material materials with Elastizitätsmodul of 208 GPa |
Flächenreduzierung | 20.0 °C | 5 - 45 % Show Material materials with Flächenreduzierung of 5 - 45 % |
Härte, Rockwell C | 20.0 °C | 32 - 37 [-] Show Material materials with Härte, Rockwell C of 32 - 37 [-] |
Streckgrenze | 20.0 °C | 692 - 830 MPa Show Material materials with Streckgrenze of 692 - 830 MPa |
Zugfestigkeit | 20.0 °C | 1103 - 1300 MPa Show Material materials with Zugfestigkeit of 1103 - 1300 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 1.41E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.41E-5 1/K | The mentioned values are between 20°C and the mentioned temperature |
600.0 °C | 1.4E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.4E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
1000.0 °C | 1.48E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.48E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
1300.0 °C | 1.53E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.53E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
Spezifische Wärmekapazität | 20.0 °C | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) | |
Wärmeleitfähigkeit | 20.0 °C | 13 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 13 W/(m·K) |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 1.1 % Show Material materials with Aluminium of 1.1 % | |
Bor | 3E-3 - 7E-3 % Show Material materials with Bor of 3E-3 - 7E-3 % | |
Chrom | 22.3 - 22.9 % Show Material materials with Chrom of 22.3 - 22.9 % | |
Eisen | 70.4 - 100 % Show Material materials with Eisen of 70.4 - 100 % | Balance |
Kobalt | 1 % Show Material materials with Kobalt of 1 % | |
Kohlenstoff | 0.03 - 0.06 % Show Material materials with Kohlenstoff of 0.03 - 0.06 % | |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % | |
Mangan | 0.2 % Show Material materials with Mangan of 0.2 % | |
Molybdän | 1.7 - 2.3 % Show Material materials with Molybdän of 1.7 - 2.3 % | |
Nickel | 55 - 58 % Show Material materials with Nickel of 55 - 58 % | |
Niobium | 0.75 - 0.95 % Show Material materials with Niobium of 0.75 - 0.95 % | |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % | |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % | |
Silizium | 0.2 % Show Material materials with Silizium of 0.2 % | |
Titan | 2.1 - 2.4 % Show Material materials with Titan of 2.1 - 2.4 % |