Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 8 % Show Material materials with Chrom of 8 % |
Eisen | 88.8 - 100 % Show Material materials with Eisen of 88.8 - 100 % |
Kohlenstoff | 0.55 % Show Material materials with Kohlenstoff of 0.55 % |
Mangan | 0.4 % Show Material materials with Mangan of 0.4 % |
Molybdän | 0.75 % Show Material materials with Molybdän of 0.75 % |
Silizium | 1.5 % Show Material materials with Silizium of 1.5 % |