Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 7.6 - 7.7 g/cm³ Show Material materials with Dichte of 7.6 - 7.7 g/cm³ | Typical for Martensitic Stainless Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 20.0 °C | 14 - 22 % Show Material materials with Dehnung A5 of 14 - 22 % | |
Elastizitätsmodul | 20.0 °C | 194 - 220 GPa Show Material materials with Elastizitätsmodul of 194 - 220 GPa | Typical for Martensitic Stainless Steel |
Flächenreduzierung | 20.0 °C | 40 - 50 % Show Material materials with Flächenreduzierung of 40 - 50 % | |
Härte, Brinell | 20.0 °C | 266 - 325 [-] Show Material materials with Härte, Brinell of 266 - 325 [-] | |
Poissonzahl | 20.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Martensitic Stainless Steel |
Streckgrenze | 20.0 °C | 750 MPa Show Material materials with Streckgrenze of 750 MPa | |
Zugfestigkeit | 20.0 °C | 1100 - 1350 MPa Show Material materials with Zugfestigkeit of 1100 - 1350 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 1.09E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.09E-5 1/K | The mentioned values are between 20°C and the mentioned temperature |
200.0 °C | 1.13E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.13E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
500.0 °C | 1.15E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.15E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
600.0 °C | 1.24E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.24E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
700.0 °C | 1.18E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.18E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
1000.0 °C | 1.32E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.32E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
1300.0 °C | 1.35E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.35E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
Schmelzpunkt | 1375 - 1450 °C Show Material materials with Schmelzpunkt of 1375 - 1450 °C | Typical for Martensitic Stainless Steel | |
Spezifische Wärmekapazität | 20.0 °C | 460 - 500 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 - 500 J/(kg·K) | Typical for Martensitic Stainless Steel |
Wärmeleitfähigkeit | 20.0 °C | 14 - 31 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 14 - 31 W/(m·K) | Typical for Martensitic Stainless Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 20.0 °C | 6E-7 Ω·m Show Material materials with spezifischer Widerstand of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 8 - 10 % Show Material materials with Chrom of 8 - 10 % |
Eisen | Balance |
Kohlenstoff | 0.4 - 0.5 % Show Material materials with Kohlenstoff of 0.4 - 0.5 % |
Mangan | 0.8 % Show Material materials with Mangan of 0.8 % |
Nickel | 0.6 % Show Material materials with Nickel of 0.6 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 2.7 - 3.3 % Show Material materials with Silizium of 2.7 - 3.3 % |