Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 7.4 - 7.7 g/cm³ Show Material materials with Dichte of 7.4 - 7.7 g/cm³ | Typical for Martensitic Stainless Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 20.0 °C | 8 - 15.5 % Show Material materials with Dehnung A5 of 8 - 15.5 % | |
Elastizitätsmodul | 20.0 °C | 194 - 220 GPa Show Material materials with Elastizitätsmodul of 194 - 220 GPa | Typical for Martensitic Stainless Steel |
Flächenreduzierung | 20.0 °C | 9 - 10 % Show Material materials with Flächenreduzierung of 9 - 10 % | |
Härte, Brinell | 20.0 °C | 293 [-] Show Material materials with Härte, Brinell of 293 [-] | |
Poissonzahl | 20.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Martensitic Stainless Steel |
Streckgrenze | 20.0 °C | 840 - 844 MPa Show Material materials with Streckgrenze of 840 - 844 MPa | |
Zugfestigkeit | 20.0 °C | 940 - 941 MPa Show Material materials with Zugfestigkeit of 940 - 941 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 200.0 °C | 9.8E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 9.8E-6 1/K | The mentioned values are between 20°C and the mentioned temperature |
600.0 °C | 1.15E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.15E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
1000.0 °C | 1.24E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.24E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
1300.0 °C | 1.31E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.31E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
Schmelzpunkt | 1375 - 1450 °C Show Material materials with Schmelzpunkt of 1375 - 1450 °C | Typical for Martensitic Stainless Steel | |
Spezifische Wärmekapazität | 20.0 °C | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) | Typical for Martensitic Stainless Steel |
Wärmeleitfähigkeit | 20.0 °C | 14 - 31 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 14 - 31 W/(m·K) | Typical for Martensitic Stainless Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 20.0 °C | 6E-7 Ω·m Show Material materials with spezifischer Widerstand of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 19 - 21 % Show Material materials with Chrom of 19 - 21 % |
Eisen | Balance |
Kohlenstoff | 0.75 - 0.9 % Show Material materials with Kohlenstoff of 0.75 - 0.9 % |
Mangan | 0.8 % Show Material materials with Mangan of 0.8 % |
Nickel | 1 - 1.7 % Show Material materials with Nickel of 1 - 1.7 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.04 % Show Material materials with Schwefel of 0.04 % |
Silizium | 1.75 - 2.6 % Show Material materials with Silizium of 1.75 - 2.6 % |