Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Medium Carbon Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 20.0 °C | 18 % Show Material materials with Dehnung A5 of 18 % | |
Elastizitätsmodul | 20.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Medium Carbon Steel |
Flächenreduzierung | 20.0 °C | 60 % Show Material materials with Flächenreduzierung of 60 % | |
Härte, Rockwell C | 20.0 °C | 35 [-] Show Material materials with Härte, Rockwell C of 35 [-] | |
Poissonzahl | 20.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Medium Carbon Steel |
Schubmodule | 20.0 °C | 75 - 80 GPa Show Material materials with Schubmodule of 75 - 80 GPa | Typical for Carbon Steel |
Streckgrenze | 20.0 °C | 960 MPa Show Material materials with Streckgrenze of 960 MPa | |
Zugfestigkeit | 20.0 °C | 1050 MPa Show Material materials with Zugfestigkeit of 1050 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 200.0 °C | 1.16E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.16E-5 1/K | The mentioned values are between 20°C and the mentioned temperature |
300.0 °C | 1.21E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.21E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
500.0 °C | 1.31E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.31E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
600.0 °C | 1.36E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.36E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
Max. Betriebstemperatur | 500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | Typical for Carbon Steel | |
Schmelzpunkt | 1380 - 1514 °C Show Material materials with Schmelzpunkt of 1380 - 1514 °C | Typical for Medium Carbon Steel | |
Wärmeleitfähigkeit | 20.0 °C | 42 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 42 W/(m·K) |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 20.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with spezifischer Widerstand of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Chemical properties
Property | Value |
---|---|
Eisen | Balance |
Kohlenstoff | 0.35 - 0.45 % Show Material materials with Kohlenstoff of 0.35 - 0.45 % |
Mangan | 1.25 - 1.75 % Show Material materials with Mangan of 1.25 - 1.75 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 0.75 % Show Material materials with Silizium of 0.75 % |